Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADILON S URV600W 339 BK - PA6-GF60 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADILON S URV600W 339 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Radilon S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
PA6 60% glass fibre reinforced injection moulding grade. Very high flowability. Heat stabilized. Black colour.

Suitable for parts requiring very high stiffness and high mechanical resistance, as in case of metal replacement applications. Excellent heat ageing properties retention.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.1 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.6 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 20800 / - MPa ISO 527
Stress at break 235 / - MPa ISO 527
Strain at break 2.1 / - % ISO 527
Charpy impact strength, +23°C 90 / - kJ/m² ISO 179/1eU
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 220 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 215 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 10.7 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 92 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E13 / 1E11 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E10 Ohm IEC 62631-3-2
Other propertiesdry / condUnitTest Standard
Water absorption 4.4 / * % Sim. to ISO 62
Humidity absorption 1.1 / * % Sim. to ISO 62
Density 1690 / - kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.15 % -
Melt temperature 240 - 280 °C -
Mold temperature 80 - 90 °C -
Diagrams
Dynamic Shear modulus-temperature , RADILON S URV600W 339 BK (dry), PA6-GF60, RadiciGroup
Stress-strain , RADILON S URV600W 339 BK (dry), PA6-GF60, RadiciGroup
Secant modulus-strain , RADILON S URV600W 339 BK (dry), PA6-GF60, RadiciGroup
Characteristics
Processing
Injection Molding
Delivery form
Granules, Black
Additives
Release agent
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
The material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.15%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. Special care must be taken to avoid moisture absorption and contamination with other polymers when adding regrind material. Colour variation and mechanical properties reduction may occur and should always be carefully monitored.

Injection Molding Processing Parameters
Melt TemperatureMold TemperatureInjection Speed
240 - 280°C80 - 90°Cmedium-High
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.